Hello Angel,
As a former PCB fabricator, I'm not sure that the base material has a shelf
life. It's usually quite stable, and lasts a very long time in the field.
Solderability, however, is a different story. Some surface finishes can
preserve solderability for many years, such as HASL (Hot Air Solder Level),
which essentially coats any exposed copper with solder. Others, such as
immersion tin and OSP (Organic Solderability Preservative), measure their
shelf life in months, weeks or days.
Hope this helps,
Bill Belanger
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|