TECHNET Archives

April 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Wed, 14 Apr 2010 18:35:49 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (86 lines)
Switch is different compare to the edge connector (No. mating time
required is much higher).  Co hardening gold may be the stuff you want,
not the Ni hardening most of the stuff used nowadays.  You need to find
someone doing the special plating for you, not share the tank of gold
for those plating for connector, zif boards, etc.  you might want to pay
for a tank...

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Wednesday, April 14, 2010 5:14 PM
To: [log in to unmask]
Subject: [TN] Question for "Old-Timers" about Gold

ya know, every time I think I know enough about a particular subject,
something comes along to make me realize there is more to it....

I need to order some boards using a fabrication drawing that hasn't been
updated in over fifteen years.
We need Hard Gold Electroplating for a rotary switch contacts.
One of the notes calls for gold knoop hardness 200-300, thickness
130-230
uin. 93.7% purity
 The last FAI report showed gold thickness of 160 uin. All other
historical
records are lost in the shifting sands of time

Our vendor has knoop hardness 150, 99.7% purity and says gold
requirement is
too thick.

IPC says knoop 150, gold minimum 31.5 uin. for edge connector fingers,
which
I assume is the same for contacts (doesn't seem to be addressed)

Printed Circuits Handbook says knoop 150,  thickness 25-50 uin for
non-military, 99.8% gold purity

Has gold plating changed that much since then?
Is there a danger of wear-out if I get 50uin. gold plating when our old
boards were 160 uin.?

surfin' the learnin' curve,
Jack


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2