DC Members:
I am designing a PCB for HAST (Highly Accelerated Stress
Testing). The customers requirements are:
DLT (150C, 408 hours)
HAST (130C, 85% RH, 96 hours)
temp cycling (-65C to 150C for devices)
on a 28 bump CSP package. (.4mm pitch, .16mm lands)
The board material recommended by some fabricators is an Arlon 35N
Polyimide, due to it's stability over temp.
My questions are...
Is this the best material without going overboard on cost?
Is there a soldermask that is very durable and can withstand this
environment. We have had problems in the past with it flaking off.
What is the tightest registration of the solder mask that I could
expect, in order to create the largest web possible between the CSP
lands. We only have .24mm between the .16mm lands.
Has anyone done this in the past and already have the formula for a
successful project?
Thanks in advance.
David Baldwin CID+
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|