We use Humiseal UV40. I thought that out, but have no data to support it
success or failure with regards to coating over a no clean flux used for
attaching through hole components that cannot go through a wash.
Jon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Thursday, March 04, 2010 4:38 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coat Over No-Clean Flux
And Doug forgot one of our favorite quotes - " Experience is what you
get
right after you need it "
Dave Hillman
Rockwell Collins
[log in to unmask]
Douglas Pauls <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/04/2010 04:17 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
Re: [TN] Conformal Coat Over No-Clean Flux
No doubt, the Technet forum tis a great thing. I seem to recall us
discussing this issue at length about a year or so ago. I suspect that
if
you search the archives, you would find the thread.
Along the lines of what you ask. While Rockwell does use low residues
fluxes (low residue is a flux, no-clean is a process) and we clean them,
we also have a very successful "reduced clean" where we solder on parts
that are either intolerant to our water wash process or it is "bloody
inconvenient (I am feeling British this afternoon). We often
conformallly
coat over those residues, usually Alpha Telecore Plus or Kester 245
)both
ROL0), successfully with Humiseal 1B31 acrylic or Humiseal 1H20AR1
acrylic-urethane. I know that you are looking at using urethanes, but
don't use those very often.
Anyone who knows Hillman or I know we test the crap out something before
we ever allow it on product, so we looked at combinations of cored wire
flux with additive fluxes, and the resultant combinations with the
coatings, mostly the solvents in the coatings which would have a
tendency
to soak into the residues, potentially altering the chemical nature of
the
resulting mix.
I think that you will largely find that solvent based coatings, such as
one part urethanes or acrylics generally adhere pretty well to low
solids
flux residues, but again, depends on the flux.
I can and does work, but like anything, ya gotta do the testing, test
drive the car, kick the tires, etc.
If'n ya knows what yur doin', life is great. If not, experience is an
expensive educator, but often very thorough.
Doug Pauls
Ken Bloomquist <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/04/2010 03:38 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ken Bloomquist <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Conformal Coat Over No-Clean Flux
Doug,
One of the great things about the TechNet is the traction you can get
from
the efforts of people who have gone before. While I know that "good"
testing
is required for every application I was hoping that I would here
something
like; "I had great results using a Xylene based Polyurethane moisture
cure
coating over ROLO no-clean flux." Or "I tried Xylene based Polyurethane
moisture cure coating over ROLO no-clean flux and it was a disaster!"
I know that my application will be a little different than anyone else's
and
require testing but was just hoping for a baseline.
KennyB
-----Original Message-----
From: Douglas Pauls [mailto:[log in to unmask]]
Sent: Thursday, March 04, 2010 1:42 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coat Over No-Clean Flux
Jon,
While that is true, that only relates to the compatibility between
fluxes.
Seldom do you have flux vendors also providing coatings. It is the
product of the combined flux residues with the coating, especially the
solvent carrier, that you have to watch out for.
Doug Pauls
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
This communication is intended only for use by the addressee(s) named herein and may contain business confidential and/or legally privileged information. If you are not the intended recipient of this e-mail, you are hereby notified that any dissemination, distribution, disclosure or copying of this e-mail and its contents is strictly prohibited. If you have received this e-mail in error, kindly notify the sender by replying to this message. In addition, please permanently delete the message and any attachments without copying or disclosing the contents. Thank you for your cooperation.
THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR DEPARTMENT OF COMMERCE.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|