Doug,
One of the great things about the TechNet is the traction you can get from
the efforts of people who have gone before. While I know that "good" testing
is required for every application I was hoping that I would here something
like; "I had great results using a Xylene based Polyurethane moisture cure
coating over ROLO no-clean flux." Or "I tried Xylene based Polyurethane
moisture cure coating over ROLO no-clean flux and it was a disaster!"
I know that my application will be a little different than anyone else's and
require testing but was just hoping for a baseline.
KennyB
-----Original Message-----
From: Douglas Pauls [mailto:[log in to unmask]]
Sent: Thursday, March 04, 2010 1:42 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coat Over No-Clean Flux
Jon,
While that is true, that only relates to the compatibility between fluxes.
Seldom do you have flux vendors also providing coatings. It is the
product of the combined flux residues with the coating, especially the
solvent carrier, that you have to watch out for.
Doug Pauls
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|