Eric,
Your question nicely leads into one that I have been pondering the last few
days - the use of Nanofoils in soldering/SMD applications. I am just
beginning to look into this but thought I might get some field experience
opinions from the forums.
One can go to the Reactive NanoTechnologies web site at
http://www.rntfoil.com/site/
At least one design realization consists of a foil created by alternating
layers of nm thick Al & Ni. Said foil would be placed between two
solder-coated surfaces, or solder performs. The foil would be ignited
[soldering iron, laser, etc] and the highly exothermic, self-propagating
reaction would locally reflow the solderable surfaces creating a bond. The
rapid exothermic process would minimize delta CTE issues between components,
leaving the bulk temperature of the components well below what they would
experience during a 'normal' reflow process.
Leaving aside for the moment, any issues related to possibly having to
physically hold the components in place during the process, I have two
predominantly material questions -
1 - Has anyone attempted to use this in a production environment yet?
2 - What happens to the strength of the joints, assuming the by-products of
the reaction stay within the interfacial region?
Just curious. Seems like a nice tool looking for an application.
Steve C
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Eric Bonatti
Sent: Thursday, March 04, 2010 11:23 AM
To: [log in to unmask]
Subject: [LF] magnetic solders?
Hello all,
Have you folks seen this?
http://www.articleant.com/gen/13521-new-magnetic-solders-are-a-leap-towards-
green-alternatives.html
I'm really curious to hear your thoughts on it.
Thanks,
Eric Bonatti, C.I.D.+
EDA and Engineering Services Group Leader
Phone: +1.905.812.6200 xt.3412
Mobile: +1.416.294.1194
E-mail: [log in to unmask]
Psion Teklogix Inc.
2100 Meadowvale Boulevard,
Mississauga, ON, L5N 7J9, Canada
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|