Hi All,
Anyone have any experience on a .001 laser via drilled through .0005 copper
and a .002 thick polyimide. The opening on the bottom side of the laser hole
is supposed to be .0004-.0006 with the taper. Can this be plated reliably?
Would an additive process make this better?
Thanks in advance. Steve Kelly
PFC_2col.png
CREATING A FLEXIBLE FUTURE
Steve Kelly
(416) 750-8433 (work)
(416) 750-0016 (fax)
(416) 577-8433 (cell)
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------