Inge, the mass of the package is probably not helping here. Have you tried
an approach such as using a low height standoff on the part and then
effectively under filling the assembly?
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Friday, March 12, 2010 10:48 AM
To: [log in to unmask]
Subject: [TN] Vibration issue
Hi all,
we are making a very vital part for a aircraft builder. Problem with TQFPs,
some 200 legs. There are resonance peaks that kill the package legs.
Redesign is not to think of from the customer, so we must do something on
inside of the box. One solution (not popular) is to use a string of a glue
along the leg rows in order to lock them. Another is to place a vibration
dampening mat on one side of the board. That one is more tricky , but there
is a US company with lots of stuff for that purpose. Anyone with
experience from this area? I should add that not all legs are broken, just
one or two after 100 hs of random vibration, but that is of course not
acceptable. BGAs would solve the problem, but there is no time for
redesign.
I'm sorry for coming with a serious message at this holy time of the week.
Thanks
/Inge
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|