This dialogue is great so far but one big part of my question is missing. I
cannot clean these solder joints with anything except spot cleaning. They
cannot go through our in-line wash. My understanding is that spot (bench)
cleaning is never a good idea as a final clean.
I understand that testing is required and I'm prepared to do that but just
wanted to get a feel for successes other people have had coating urethane
over no-clean.
By the way Inge, I'm not trying to cut corners by putting on no-clean pants
;-)
Thanks,
KennyB
-----Original Message-----
From: Inge [mailto:[log in to unmask]]
Sent: Thursday, March 04, 2010 11:02 AM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coat Over No-Clean Flux
Who would like to live with no-clean pants? Cleanliness is alpha and omega
even for electronics. I'm not a friend of NC either. I've never understood
why this was introduced. Do you really save lots of money? Who is guilty?
AT&T? or Bell? or Motorola? At least, I'm sure it was not Brian Ellis. He
wears clean pants... oh.. it's not Friday yet.
Inge
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|