There is a 150 micro inch layer of nickel under the electroless gold.
Regards Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: March-31-10 3:50 PM
To: [log in to unmask]
Subject: Re: [TN] Wire bondable gold
You encapsulate traces/pads with Electroless Gold and eliminate future
contaminations due to copper/nickel corrosion I guess.
------Original Message------
From: Steve Kelly
Sender: TechNet E-Mail Forum.
To: TechNet E-Mail Forum.
ReplyTo: TechNet E-Mail Forum.
ReplyTo: Steve Kelly
Subject: [TN] Wire bondable gold
Sent: Mar 31, 2010 3:20 PM
Hi all,
Anyone know a reason why a customer would call up 20 micro inches of
electroless gold followed by 50 micro inches of electroplated soft gold for
thermosonic gold wire bonding? Is there an advantage to having the
electroless underneath?
Regards Steve Kelly
PFC_2col.png
CREATING A FLEXIBLE FUTURE
Steve Kelly
(416) 750-8433 (work)
(416) 750-0016 (fax)
(416) 577-8433 (cell)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Regards
Aleks Lozinsky
Technical Sales Representative
Technic Canada Inc.
Office: 905-940-4020
Cell: 416-450-1093
E-mail: [log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|