TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 2 Mar 2010 15:59:12 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Subject:
From:
Ioan Tempea <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (141 lines)
Nevermind the salary this lady makes, the difference is certainly cashed by the engineer who required this.

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask] 
W | www.digico.cc

N'imprimer que si nécessaire - Print only if you must


-----Message d'origine-----
De : Lee parker [mailto:[log in to unmask]] 
Envoyé : March-02-10 3:37 PM
À : [log in to unmask]
Objet : Re: [TN] Unusual Assembly Requirement...

Steve

I do not know how much you are paying this lady, except it's not enough.

Best regards
Lee
J. L. Parker Ph. D.
JLP Consultants LLC
804 779 3389
  ----- Original Message ----- 
  From: Nowland, Russell Howard (Russell)<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Tuesday, March 02, 2010 3:10 PM
  Subject: Re: [TN] Unusual Assembly Requirement...


  This is insane!!!!!

  Russell Nowland
  Alcatel-Lucent
  Advanced Manufacturing Engineer
  Address: 14000 Quail Spring Parkway, Suite 300
  Oklahoma City, OK 73134
  email: [log in to unmask]<mailto:[log in to unmask]>
  Desk: 405-302-1660
  Cell: 405-203-0034
  Fax: 405-302-1622

  -----Original Message-----
  From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
  Sent: Tuesday, March 02, 2010 1:52 PM
  To: [log in to unmask]<mailto:[log in to unmask]>
  Subject: [TN] Unusual Assembly Requirement...

  Hi All,



  I came into work today and saw something that I've not seen before. Keep in
  mind that the area shown is about ½" square, and that these are 0402's...



  http://stevezeva.homestead.com/files/Quad_Stack.JPG<http://stevezeva.homestead.com/files/Quad_Stack.JPG>



  This was done using two reflows, and the caps were not touched by a
  soldering iron.



  You may ask why. It's because it's what we were asked to do by our customer.



  We have a very talented lady working on the production floor who
  accomplished this.



  Steve


  ______________________________________________________________________
  This email has been scanned by the MessageLabs Email Security System.
  For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
  ______________________________________________________________________

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 15.0
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

  ______________________________________________________________________
  This email has been scanned by the MessageLabs Email Security System.
  For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]> 
  ______________________________________________________________________

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 15.0
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2