TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 2 Mar 2010 15:11:47 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
<001901caba41$d84e2140$88ea63c0$@com>
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (92 lines)
 Hi Steve,
A 3-D model of Manhattan——must be a RF design.

Werner
Upcoming workshops:
May 21, IPC Int. Conference on Reliability and Quality of Lead-Free Electronics, Frankfurt, Germany,
      “Reliability Issues and Solution Options for Pb-Free Soldered Electronic Products”
May 26, FED Seminar, Stuttgart, Germany,
     “Bleifreie Lötprozesse—Frühausfälle, Qualität, Zuverlässigkeit”
June 8, SMT/HYBRID/PACKAGING 2010, Nürnberg, Germany,
     “Reliability Issues with Lead-Free Soldering”



 

 

-----Original Message-----
From: Steve Gregory <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Mar 2, 2010 2:52 pm
Subject: [TN] Unusual Assembly Requirement...


Hi All,

 

I came into work today and saw something that I’ve not seen before. Keep in
mind that the area shown is about ½” square, and that these are 0402’s…

 

http://stevezeva.homestead.com/files/Quad_Stack.JPG

 

This was done using two reflows, and the caps were not touched by a
soldering iron. 

 

You may ask why. It’s because it’s what we were asked to do by our customer.

 

We have a very talented lady working on the production floor who
accomplished this.

 

Steve


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

 
=

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2