I don't know why you would want to re-ball. I initially was concerned about soldering to this alloy with eutectic SnPb, but Tech-Netters convinced me that there was no problem, and indeed there was not!
The high Pb balls act as nice standoffs to keep the joint height up. Only part which requires imagination is printing solder paste to place them into, and that's only if it's a flipchip.
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Wednesday, March 10, 2010 5:31 PM
To: [log in to unmask]
Subject: Re: [TN] 90Pb / 10Sn SOLDER BALLS
Hi Lee,
That is about right-for larger BGAs you may have to run the peak reflow zone somewhat hotter-you need to reach 203C for about 5 sec at the solder ball centermost under the BGA.
Werner
-----Original Message-----
From: Lee Whiteman <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, Mar 10, 2010 5:14 pm
Subject: [TN] 90Pb / 10Sn SOLDER BALLS
If you had to re-ball a BGA with 90Pb/10Sn non-collapsible solder balls, what
would your peak temperature be? For reflow soldering processing purposes, what
would your peak temperature be?
If it was eutectic SnPb, I would anticipate the peak temperature to be about
215C for re-balling and reflow soldering.
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|