I really dislike the term "activation", it's misleading.
The activators used in "no-clean" fluxes (and Dave Hillman really prefers
"low-solids") are typically dicarboxylic acids that will volatilize at
soldering temperatures, so several seconds at 220-260C usually drives off
enough dicarboxylic acid that the flux residue remaining on the board is
relatively safe with respect to electrochemical failure modes in most
service environments. The amount of time at a certain temperature depends
on the particular flux being used. However , the flux residue is not the
only things on boards that can have a deleterious effect on reliability.
Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069
Leland Woodall wrote:
Everyone,
To what temperature and duration must typical no-clean fluxes be exposed
before they are activated and be safely left on the board?
I've tried to contact Alpha to answer this, but haven't been able to
speak with a single technical rep all morning...
Thanks,
Leland
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|