TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 25 Mar 2010 11:56:29 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Joseph E (US SSA)" <[log in to unmask]>
Subject:
From:
"Kane, Joseph E (US SSA)" <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (110 lines)
Here's a pretty good scan:

http://ipc-technet.groupsite.com/galleries/photo/117591

-Joe

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US SSA)
Sent: Thursday, March 25, 2010 11:34 AM
To: [log in to unmask]
Subject: Re: [TN] Orange Peel Termination Finish

Not blumpy exactly.  I don't have a soft copy of this document, so I'm trying to get a good scan.

-Joe 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Thursday, March 25, 2010 11:14 AM
To: [log in to unmask]
Subject: Re: [TN] Orange Peel Termination Finish

Eeeeewwwww... That is ugly!

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, March 25, 2010 10:43 AM
To: [log in to unmask]
Subject: Re: [TN] Orange Peel Termination Finish

Does it look something like this?

http://stevezeva.homestead.com/files/Connector_Blumpies.jpg

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US SSA)
Sent: Thursday, March 25, 2010 9:38 AM
To: [log in to unmask]
Subject: [TN] Orange Peel Termination Finish

One of our guys brought over a counterfeit parts manual with a picture of some component leads exhibiting a rough orange-peel texture.  The picture was presented as evidence of re-tinning, which could indicate a counterfeit part.

The question is what could cause orange peel finish after hot solder dip?  We perform a lot of hot solder dip, both in-house and outside, and neither of us could remember the last time we saw anything like this, though it does look kind of familiar.

In the picture, we could see no obvious patches of de-wetting or non-wetting, just a uniform pebbly surface.  I don't think this would be caused by a solderability problem, or rapid cooling, could it be too little immersion time in the hot solder?  Could the solder in the pot be contaminated with something like copper, gold, or iron?

-Joe


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender.  If you have received this email in error, please immediately return it to sender and delete the copy you received.



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2