I add this : we have tried to grow Tin whiskers on pure Tin objects and also
on Immersion Tin without success. Tried biasing, cold, heat, humidity,
storage, but nothing ever happened. I've myself had a look at some objects
for years (!) but never succeeded to produce any whiskers. But I've
investigated several cases from the field. I sent one such example to NASA
from a waveguide filled with up to 10 mm long whiskers. I took a similar
waveguide and ran tests, nothing happened . Seems like they are hard to
predict. Spoky things.
Inge
--------------------------------------------------
From: "Inge" <[log in to unmask]>
Sent: den 24 March 2010 14:07
To: <[log in to unmask]>
Subject: Re: [TN] Tin Whiskers
> Hi Steve,
>
> I know you are a experienced person. How come you ask? Do I
> misunderstand something in your lines. You know well that there are
> hundreds of papers on Tin whiskers in conjunction with Immersion Tin.
>
> Jay, are you there? You are the best in the US on this topic. Can you
> open Pandora's box? I've lots of material, but as the Great King of
> Whiskers, you ought to say something.
>
> During the time waiting for Jay, you can read this one:
>
> http://www.atotech.com/fileadmin/pdf/papers/el/Immersion_tin_and_tin_whisker_growth.pdf
>
> Inge
>
>
>
>
>
>
> --------------------------------------------------
> From: "Steve Kelly" <[log in to unmask]>
> Sent: den 24 March 2010 10:30
> To: <[log in to unmask]>
> Subject: [TN] Tin Whiskers
>
>> Hi All,
>>
>> Two questions today:
>>
>> 1) Any known instances of tin whiskering when the finish is
>> Immersion Tin
>>
>> 2) Any known instances of tin whiskering after the immersion tin is
>> soldered with a RoHS compliant solder such as SAC 305.
>>
>> Thanks. Steve Kelly
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>
>>
>> PFC_2col.png
>>
>> CREATING A FLEXIBLE FUTURE
>>
>>
>>
>> Steve Kelly
>>
>> (416) 750-8433 (work)
>>
>> (416) 750-0016 (fax)
>>
>> (416) 577-8433 (cell)
>>
>>
>>
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>> ext.2815
>> -----------------------------------------------------
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|