Gregg,
It depends. There are a wide range that we use, depending on the
application and the customer requirements. We use several silicones, but
those may not meet the outgassing requirements for space. We have some
urethanes, but they may not have the flammability characteristics required
by FAA for commercial flight hardware. We have some other adhesives, but
may not meet the fungus resistance reqiurements for military applications
(hence my recent question). Epoxies are very nice, unless you want to
rework them, then they ain't.
The most frightening comment I ever heard came from a senior VP in design
engineering who asked why don't we just use materials with no drawbacks.
For one of the few times in my life, I was speechless. Leave it alone
Dewey.
Doug Pauls
Gregg Owens <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/10/2010 11:19 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Gregg Owens <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Component Staking Adhesive
Dear Technetters:
A general survey question as to what type of adhesive you use to stake
components to survive Aerospace/Space applications?
Thanks in advance.
Gregg Owens
Technical Writer - Avionics
Space Exploration Technologies
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|