I think we have to include this criteria in the 2221/2222 where
appropriate. Otherwise designers will not consider this in their design.
6012 can only address defect criteria, not attempt to backfeed design
criteria.
Gary Ferrari
FTG Circuits
Director, Technical Support
860-350-9300
On 3/16/2010 8:11 AM, Thomas E Kemp wrote:
> The design controls how close the conductors are to the edge and what
> material is used. The results of those two inputs require the fabricator
> to modify their process to compensate for the design. Often, fabrication
> modifications can not provide the needed results.
> Tom Kemp
> Sr QAE
> Rockwell Collins
> 319-295-1619
>
>
>
> "Gandhi, Mahendra S (AS)"<[log in to unmask]>
> Sent by: IPC-600-6012<[log in to unmask]>
> 03/15/2010 10:00 PM
> Please respond to
> "(Combined Forum of D-33a and 7-31a Subcommittees)"<[log in to unmask]>
>
>
> To
> [log in to unmask]
> cc
>
> Subject
> Re: [IPC-600-6012] Edges and Crazing/Haloing
>
>
>
>
>
>
> I would call it as a design, material and/or fabrication combo.
>
> Mahendra Gandhi
>
> -----Original Message-----
> From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Thomas E
> Kemp
> Sent: Monday, March 15, 2010 8:25 AM
> To: [log in to unmask]
> Subject: Re: [IPC-600-6012] Edges and Crazing/Haloing
>
> With the new high temp materials we are finding haloing popping up where
> we never were before. It is still a design issue.
> Tom Kemp
> Sr QAE
> Rockwell Collins
> 319-295-1619
>
>
>
> Mike Hill<[log in to unmask]>
> Sent by: IPC-600-6012<[log in to unmask]>
> 03/15/2010 10:09 AM
> Please respond to
> "(Combined Forum of D-33a and 7-31a Subcommittees)"<[log in to unmask]>
>
>
> To
> [log in to unmask]
> cc
>
> Subject
> Re: [IPC-600-6012] Edges and Crazing/Haloing
>
>
>
>
>
>
> Jim is headed in the right direction.
>
> All of the issues I have with haloing are with polyimide material. If this
>
> is universal, we might modify requirements by material type.
>
> Mike Hill
> Quality Manager
> Colonial Circuits, Inc.
> 540-752-5511 x121
>
> -----Original Message-----
> From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Monarchio,
> James
> Sent: Monday, March 15, 2010 9:58 AM
> To: [log in to unmask]
> Subject: Re: [IPC-600-6012] Edges and Crazing/Haloing
>
> John - this still does not resolve the issue we parked.
> The design can have spacing such that no crazing, etc. is allowed. We
> discussed (and parked) verbiage relating the requirement to designs that
> comply with 2221.
>
> Wendy's example may indeed be unmaunfacurable to the spec (and I agree).
> In practice these issues are given a blind eye until there is an issue of
> some type then parts that were acceptable yesterday are noncompliant
> today. This is a bad situation for all.
>
>
> I believe we should define a hard crazing allowance for product not
> designed to 2221 (i.e. 10 mils)- it would be neater and cleaner as well as
>
> getting the real issue back where it belongs - design.
>
> Jim
> -----Original Message-----
> From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of John Perry
> Sent: Sunday, March 14, 2010 5:06 PM
> To: [log in to unmask]
> Subject: Re: [IPC-600-6012] Edges and Crazing/Haloing
>
> Jack and All,
>
> We used to say the following in 3.3.1, Edges, in IPC-6012B:
>
> 3.3.1 Edges - Nicks, crazing or haloing along the edge of the board, edge
> of cutouts and edges of nonplated-through holes are acceptable provided
> the penetration does not exceed 50% of the distance from the edge to the
> nearest conductor or 2.5 mm [0.0984 in], whichever is less.
>
> Now IPC-6012C will say the following:
>
> 3.3.1 Edges - Nicks or crazing along the edge of the printed board, edge
> of cutouts and edges of non-plated holes are acceptable provided the
> penetration does not exceed 50% of the distance from the edge to the
> nearest conductor or 2.5 mm [0.0984 in], whichever is less. The distance
> between the haloing penetration and the nearest conductive feature shall
> not be less than the minimum lateral conductor spacing, or 100 µm [3,937
> µin] if not specified.
>
> Regards,
>
> John Perry
> Technical Project Manager
> IPC - Association Connecting Electronics Industries®
> 3000 Lakeside Drive # 309S
> Bannockburn, IL 60015-1249 USA
> +1 847-597-2818 (tel)
> +1 847-615-7105 (fax)
> +1 847-615-7100 (Main)
> [log in to unmask]
> www.ipc.org
>
>
>
> -----Original Message-----
> From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Jack Olson
> Sent: Friday, March 12, 2010 3:25 PM
> To: Listserv IPC-600-6012
> Subject: Re: [IPC-600-6012] Edges and Crazing/Haloing
>
> The guideline for edge to hole is in IPC-2222, not IPC-2221
> in IPC-2222 10.1.1 it says board edge or unplated hole to conductor
> shall not be less than Table 6-1 of IPC-2221 plus .4mm
> (and Table 6-1 is your minimum clearance based on voltage)
>
> The MINIMUM from Table 6-1 (.05mm) plus .4mm works out to 17mils!
>
> The discussion you remember was regarding IPC-2222 requirement
> for haloing, and I'm not sure it was ever resolved, but I remember
> we DID change some wording for the next revision.
> You could get the new changes from John Perry for your own interest,
> but of course it won't mean much until it is officially published.
>
> And the haloing rule it won't help if your designers are disregarding the
> clearance guideline, but I'm sure you know THAT (grin)
> good luck!
> Jack
> On Fri, Mar 12, 2010 at 10:11 AM, Wendi Boger<[log in to unmask]>
> wrote:
>
>
>> Everyone,
>>
>>
>>
>> I seem to remember a discussion about Haloing of edges and non plated
>> holes at one of our recent meetings. The requirement for the haloing
>> to be less than 50% the distance to nearest conductor works assuming the
>> design has a reasonable space from conductor to edge. I looked in
>> IPC2221 but did not find a guideline for suggested minimum distance. We
>> are seeing non-plated tolling holes with surface ground rings at<10mils
>> hole edge to copper. Depending on the material and hole size it's
>> difficult to meet the 50% rule.
>>
>>
>>
>> Is there a section in 2221 I can send the designers to so we can
>> avoid this type of issue?
>>
>>
>>
>> Thanks,
>>
>> Wendi Boger
>>
>>
>>
>>
>>
>> This communication is for use by the intended recipient(s) only and may
>> contain information that is privileged, confidential, proprietary and
>>
> exempt
>
>> from disclosure under applicable law. You are hereby notified that any
>> dissemination, distribution, forwarding or copying hereof is strictly
>> prohibited without the express written consent of DDi. If you have
>>
> received
>
>> this communication in error or are not the intended recipient, you
>>
> should
>
>> destroy the message and any attachments or copies, and you are
>>
> prohibited
>
>> from retaining, distributing, disclosing, or using any information
>>
> contained
>
>> herein. Please inform us of the erroneous delivery by return e-mail.
>>
> Thank
>
>> you for your cooperation.
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or
>>
> [log in to unmask]
>
>> ______________________________________________________________________
>>
>>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> NOTICE: This email message is for the sole use of the intended
> recipient(s) and may contain confidential and privileged information. Any
>
> unauthorized review, use, disclosure or distribution is prohibited. If
> you are not the intended recipient, please contact the sender by reply
> email and destroy all copies of the original message.
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
>
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]