Dear Dave:
J-STD-001's only exception to gold tinning is ENIG plated PCBs. Also it provides that the entire requirement be ignored if you have data to support that no gold embrittlement issues exist without pre-tinning.
Gregg Owens
Technical Writer - Avionics
Space Exploration Technologies Corporation
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave He
Sent: Thursday, February 04, 2010 12:19 PM
To: [log in to unmask]
Subject: [TN] Tinning gold-plated solder cup of connectors
Does gold plated solder cup of connector need tinning per J-STD-001? Or is
this a exemption? Thanks.
Best regards,
Dave He
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------