Change the Pb to Sn and you have a standard Sn/Ag eutectic. Makes more
sense methinks..........
Regards
Ian Fox
Lead Materials and Process Engineer
Aero Engine Controls
A Rolls-Royce plc and Goodrich Corporation Joint Venture
York Road
Hall Green
Birmingham B28 8LN
Tel: +44 90)121 607 3763
Fax: +44 900121 6076358
email: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: 11 February 2010 20:32
To: [log in to unmask]
Subject: Re: [TN] Old reference for silver solder - what's it cross ref
to?
Hi Jeff - I do have a 95Pb/5Ag solder alloy in my solder alloy charts
but don't have a 94Pb/6Ag. But your logic makes the most sense so far.
Dave
"McGlaughlin, Jeffrey A" <[log in to unmask]> Sent by: TechNet
<[log in to unmask]> 02/11/2010 01:45 PM Please respond to TechNet E-Mail
Forum <[log in to unmask]>; Please respond to "McGlaughlin, Jeffrey A"
<[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Old reference for silver solder - what's it cross ref to?
I think the 94LTS was the designation for "Low Temperature Silver
Solder"
and was 94Pb/6Ag. I have an old chart for this somewhere but can't lay
hands on it right now.
Jeffrey A McGlaughlin, CID
Engineering Designer
Battelle
505 King Ave
Columbus Ohio 43201-2693
Phone (614)424-7582
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Thursday, February 11, 2010 2:24 PM
To: [log in to unmask]
Subject: Re: [TN] Old reference for silver solder - what's it cross ref
to?
Hi Graham - well, ya got me stumped. I have access to all of the
QQ-S-571
revisions from "B" and there is no "94" designation in the
specification.
That drawing note has to newer than QQ-S-571 Rev C, 1963, since that's
when the R-RMA-RA convention was first used. The WRAP3 is easy - wire,
RA
flux, P3 flux core but the 94 LTS is a mystery. If I had to guess, the
94
LTS is a specific supplier alloy designation that has nothing to do with
the 571 specification. And the "silver solder" reference is no help as
that could be describing a solder alloy family or could be a slang term.
Looks like someone created a drawing note mutation! Good Luck.
Dave
Graham Collins <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/11/2010 11:42 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] Old reference for silver solder - what's it cross ref to?
Hello Technet
I seem plagued with strange solder questions these days. Can somebody
help with a cross-reference from an old solder callout to what this
would be referred to as now? I have a drawing that references:
"QQ-S-571 alloy 94LTS Type WRAP3", and refers to it as "silver solder".
I can get the last version of QQ-S-571 (rev F, before it was cancelled
and J-STD-006 adopted), but I do not see this type of callout. Does
anyone have something that will tell me what's in this solder?
Thanks!
Graham Collins
Halifax Production Engineering
L-3 Communications ES
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
--------------------------------------------------------------------------
This message (and any attachment) is confidential and is intended for the named recipient only.
If you receive it in error please e-mail back the sender and permanently delete the original message and any copies.
Rolls-Royce Goodrich Engine Control Systems Limited.
Registered Office: Moor Lane, PO Box 31, Derby, DE24 8BJ.
Registered in England No. 06686268.
--------------------------------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|