LoL
-----Original Message-----
From: Hernefjord Ingemar [mailto:[log in to unmask]]
Sent: 25 February 2010 08:09
To: TechNet E-Mail Forum; Rex Waygood
Subject: RE: [TN] Hackneyed?
Sorry, missed to tell you all. Had to sputter some nanometers of Gold on
the samples to avoid charging up when doing SEM. So, omit Gold.
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Waygood
Sent: torsdag 25 februari 2010 08:59
To: [log in to unmask]
Subject: Re: [TN] Hackneyed?
I just sat and looked at your images and the documents.
Why are you seeing so much Gold on your pads?
That would not seem to be good.
Regards
Rex
Rex Waygood
Technical Manager
Hansatech EMS provides value manufacturing through engineering and
quality
Hansatech EMS Limited
Benson Road
Nuffield Industrial Estate
Poole
Dorset
BH17 0RY
+44 (0)1202 338200
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: 24 February 2010 19:54
To: [log in to unmask]
Subject: [TN] Hackneyed?
Hi Folks,
am asking you to sacrifice a minute on a topic that may make you sick,
as much as it has been discussed. Have a look at the SEM images that
(hopefully) will be beamed by our most honorable guy, Dr Gregory. By
order:
1. Pic 38 BGA ball after the preying off the 560 ball BGA from the
board.
SEI mode.
2. pic 39, same at x 5,000
3. pic 40,samet at x 10,000
4.pic, 41 same at x 20,000
These four show the face of the pulled-off balls. The package/board was
sectioned into halv by half inch pieces with a thin blade diamond saw
and then each BGA section was separated from the board by means of a
steel.
After SEM 1-4 I made EDS, which can be seen below.
5. XILINX_backlund_ball_2.doc
As you can see, there is nearly no Lead (!), a high w/% Nickel, a little
Tin and lots of Phosphorous. Clearly, the separation has been in a
Sn/Ni/P-layer.
Now, continue with having a look at the board pads after the
preying-off.
6. pic 44, Board pad at low magnification and SEI mode.
7.pic 46, same at x 5,000
8.pic 48, same at x 10,000
9. pic 50, same at x 20,000
10. pic 51, same but with BS mode
11. XILINX_backlund_pad_1.doc
As you can see here, there is more Lead, a high w/% Nickell, much more
Tin and still lots of Phosphorous.
Discussion:
Obviously, real and reliable solder joints are only in the
circumperipheric of the whole (best understood with pic 10). How strong
the adhesion was in the main part of the joint, we don't know. From the
function (final) electrical testing, we have experienced several cases
with disturbed signals. Many a times, we have had to remove the BGA and
supersede with a fresh one. The test engineer told me, that by slightly
add pressure to the BGA, he may get the signal through again. He thinks
we have an issue with the uvias, others think there is a problem with
the BGAs, myself I'm committed to my theory that this has to do with the
rotten interface between the Tin/Lead and the ENIG pads.
Question:
Is anyone familiar with the said? What is your opinion about the
demonstrated solder joints? Can yoy get cracks and electrical
misfunction, despite that hundreds of balls are holding the BGA close to
the board in a 'iron grip' ?
Wayne? Steve? Dave? George W? Vlad?
Thanks in advance. You'll have to wait for Steve to fix the exhibition.
/Inge
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|