"With tin whiskers, absence of evidence is seldom evidence of absence,
the remaining whiskers are usually evident."
Fair enough. And, indeed, there is potentially more evidence of this
type of failure in spaceborne equipment where substantial arcing can occur.
(I think Bob did a good job of encapsulating the rest in his latest post.)
What a great community --
--- Previous Message in This Thread ---
Subject: Re:[LF] Perfect opportunity for tin whiskers induced failures -
Toyota did not install brake override systems despite complaints
From: Stadem, Richard D. <[log in to unmask]>
To: [log in to unmask]
Date: Tuesday, February 02, 2010 12:18:05 PM
> That is not completely true.
> While the solitary whisker or whiskers on an electronic device that
> caused the short leading to overvoltage or non-conforming signal
> conditions may burn itself away in our atmosphere, several more shorter
> non-conducting whiskers are usually left behind. With tin whiskers,
> absence of evidence is seldom evidence of absence, the remaining
> whiskers are usually evident.
> In space, a tin whisker acts the same as a filament in a light bulb, due
> to the vacuum (lack of oxygen). In that situation a short is usually
> permanently fused between the adjacent non-common conductors, and while
> it may break off during re-entry, enough evidence usually, but not
> always, is left behind to make a determination as to what happened.
>
> -----Original Message-----
> From: Leadfree [mailto:[log in to unmask]] On Behalf Of Marcus L. Thompson
> Sent: Tuesday, February 02, 2010 2:07 PM
> To: [log in to unmask]
> Subject: Re: [LF] Perfect opportunity for tin whiskers induced failures
> - Toyota did not install brake override systems despite complaints
>
> "...tin whiskers are a convenient thing liabilitywise for manufacturers
> in any violent catastrophe involving same: They can simply break off and
>
> fall away from the scene of the crime, all without a trace."
>
> Is this at all true?
>
> If so, who's to say what actually happened? Could human nature possibly
>
> factor in to the statements and proclamations of a large industrial
> organization when confronted with an accusatory public eye?
>
> Tin whiskers are yet another failure vector for these systems; one which
>
> is increasingly likely to meaningfully assert itself in devices
> manufactured using lead-free technologies with the passage of time.
>
> So, perhaps one could say it's all a matter of time...
>
>
>
> --- Previous Message in This Thread ---
> Subject: Re:[LF] Perfect opportunity for tin whiskers induced failures -
>
> Toyota did not install brake override systems despite complaints
> From: John Burke <[log in to unmask]>
> To: [log in to unmask]
> Date: Tuesday, February 02, 2010 8:57:21 AM
>
>> They also stated publicly a few months ago that the problem was floor
>> mats......8-)
>>
>>
>> John Burke
>> (408) 515 4992
>>
>>
>> -----Original Message-----
>> From: Leadfree [mailto:[log in to unmask]] On Behalf Of TIMOTHY MCGRADY
>> Sent: Tuesday, February 02, 2010 7:42 AM
>> To: [log in to unmask]
>> Subject: Re: [LF] Perfect opportunity for tin whiskers induced
> failures -
>> Toyota did not install brake override systems despite complaints
>>
>> Toyota stated publicly today that the cause was not electronic in
> nature.
>> -----Original Message-----
>> From: Leadfree [mailto:[log in to unmask]] On Behalf Of Pete Houwen
>> Sent: Tuesday, February 02, 2010 9:24 AM
>> To: [log in to unmask]
>> Subject: Re: [LF] Perfect opportunity for tin whiskers induced
> failures -
>> Toyota did not install brake override systems despite complaints
>>
>> the electronic controlled throttle also makes traction control far
> easier to
>> implement. Since loss of traction is far more common than stuck
> throttles,
>> they saved money and increased safety.
>>
>> Of course, including a "brake wins" algorithm would have saved lives.
> And
>> amortized over millions of cars, software is almost free.
>>
>> I don't know if Toyota has nailed the problem with the friction
> solution.
>> But it
>> has been vetted by the NHTSA, and they seem to agree. I don't doubt
> there
>> is also an electronic failure problem - electronics fail. But what I
> do
>> know is there is no indication so far of a tin whisker problem. It
> concerns
>> me that
>>
>> blaming any electronic failure on tin whiskers without any scientific
>> evidence is really no more valid than banning lead in solder with no
>> scientific evidence.
>> There's enough data, crying wolf won't get RoHS repealed. That's more
>> likely to just make it harder to stop the next legislative mistake.
>>
>>
> ------------------------------------------------------------------------
> ----
>> ---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
> To
>> unsubscribe, send a message to [log in to unmask] with following text in
> the
>> BODY (NOT the subject field): SIGNOFF Leadfree To temporarily
> stop/(start)
>> delivery of Leadree for vacation breaks send:
>> SET Leadfree NOMAIL/(MAIL)
>> Search previous postings at: http://listserv.ipc.org/archives Please
> visit
>> IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at
> [log in to unmask] or
>> 847-615-7100 ext.2815
>>
> ------------------------------------------------------------------------
> ----
>> ---
>>
>>
> ------------------------------------------------------------------------
> ----
>> ---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
> To
>> unsubscribe, send a message to [log in to unmask] with following text in
> the
>> BODY (NOT the subject field): SIGNOFF Leadfree To temporarily
> stop/(start)
>> delivery of Leadree for vacation breaks send: SET Leadfree
> NOMAIL/(MAIL)
>> Search previous postings at: http://listserv.ipc.org/archives Please
> visit
>> IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional
>> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
>> ext.2815
>>
> ------------------------------------------------------------------------
> ----
>> ---
>>
>>
> ------------------------------------------------------------------------
> -------Leadfee Mail List provided as a service by IPC using LISTSERV
> 1.8d
>> To unsubscribe, send a message to [log in to unmask] with following text
> in
>> the BODY (NOT the subject field): SIGNOFF Leadfree
>> To temporarily stop/(start) delivery of Leadree for vacation breaks
> send: SET Leadfree NOMAIL/(MAIL)
>> Search previous postings at: http://listserv.ipc.org/archives
>> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> ------------------------------------------------------------------------
> -------
>
> ------------------------------------------------------------------------
> -------Leadfee Mail List provided as a service by IPC using LISTSERV
> 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop/(start) delivery of Leadree for vacation breaks
> send: SET Leadfree NOMAIL/(MAIL)
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> ------------------------------------------------------------------------
> -------
>
> -------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Leadfree
> To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
> Search previous postings at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -------------------------------------------------------------------------------
>
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|