Does anyone have any information regarding crack propagation? A bare
board is allowed to have laminate cracks as long as they are in the
non-evaluation zone or if they originate in the non-evaluation zone they
can't be longer than 3 mils going into the evaluation zone.
What is the requirement or what should I expect to see after the bare
board has been assembled and run through thermal cycle and vibration
testing? Should there be no propagation or ???
Thanks,
Pete Menuez