Well, it depends. Depends on the coating used and how tied you are to
cosmetics. Usually, the chemicals used to strip the coating for rework
clean the rework site as well. When these flux removers are used to
remove the flux from rework, it might affect the gloss of the coating, but
for the coatings we used, we determined that it was cosmetic only, not a
functional degradation. But it depends on the coatings used.
Doug Pauls
Ioan Tempea <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/10/2010 07:50 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Ioan Tempea <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Cleaning for Hand Soldering
Doug,
Can the substances you've mentioned be used in the repairs of conformal
coated assemblies?
Thanks,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask]
W | www.digico.cc
N'imprimer que si nécessaire - Print only if you must
-----Message d'origine-----
De : Douglas Pauls [mailto:[log in to unmask]]
Envoyé : February-10-10 8:32 AM
À : [log in to unmask]
Objet : Re: [TN] Cleaning for Hand Soldering
Bob,
As I have told many a person here, isopropyl alcohol SUCKS as a cleaner.
Sucks sucks sucks. Horrid. Awful. Rotten. I could go on, but seem to
have misplaced my thesaurus.
I would recommend either Chemtronics Heavy Duty Flux Off (yes, that is an
actual name) or Kyzen's Cybersolv 141R.
Doug Pauls
bob wettermann <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/10/2010 06:29 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
bob wettermann <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Cleaning for Hand Soldering
Technetters:
Can you a please weigh in on the following question .....
One of our customers' hand soldering processes uses Kester 186
rosin liquid flux=A0 along with SN63/PB37=A0 rosin core solder. They
currently use 99% isopropyl alcohol for cleanin and want to get away from
this method.
The options being considered are:
1) Kontakt PCC (out of Europe)
2) Ecoline Techspray
Does anyone have any experience with either product good or bad?
Thanks!!
Bob Wettermann
BEST Inc
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|