TECHNET Archives

February 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Dave He <[log in to unmask]>
Date:
Thu, 4 Feb 2010 18:24:44 -0600
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Dean Stadem <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
Analog Technologies Corp
MIME-Version:
1.0
Parts/Attachments:
text/plain (161 lines)
J-STD-001DS specifically does not allow ANY gold on areas to be
soldered, except for ENIG on circuit boards, and ENIG only as defined
per IPC 4552.
Objective evidence is also not considered to be immediate pull or peel
test readings, because gold embrittlement is a time-variable phenomena.
Gold cups have been proven to be especially susceptible to brittle
fractures from gold nucleation over time. I had to deal with that when
several wires broke from vibration inside of torpedoes, so I know they
are especially vulnerable. The gold content in the solder was proven to
be less than 2%.
I am sure Werner will weigh in on this as well.

R. Dean Stadem
Consulting Engineer
Analog Technologies Corp./Lumagine, Inc.
11441 Rupp Drive
Burnsville, MN 55431
(952)894-9228
[log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave He
Sent: Thursday, February 04, 2010 5:54 PM
To: [log in to unmask]
Subject: Re: [TN] Tinning gold-plated solder cup of connectors

Great, Bob. This is what I am looking for. Two Qs

1. The amendment is for J-STD-001 DS, will it cover J-STD-001?
2. Does " Surfaces exhibiting gold finish thicknesses of 0.254
micro-meters
(10 micro-inch) or less (a.k.a. ''gold-flash'') are exempt from this
requirement." cover SMT component? I guess so but it not clearly stated.

Thanks.

Regards,
 
Dave He
Ext: 333
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Landman
Sent: Thursday, February 04, 2010 2:34 PM
To: [log in to unmask]
Subject: Re: [TN] Tinning gold-plated solder cup of connectors

Gold flash is also exempt according to the amendment #1 of J-STD-001DS -
isn't the SAMTEC part gold flash?

http://www.ipc.org/4.0_Knowledge/4.1_Standards/J-STD-001DS-Amend1.pdf

3.9.3 Gold Removal Gold shall be removed from at least 95% of the
surface
to-be-soldered of all component leads,
component terminations, and solder terminals. A double tinning process
or
dynamic solder wave may be used for
gold removal.

Exceptions:

Electroless nickel immersion gold (ENIG) finishes on PCBs are exempt
from
this requirement.
Surfaces exhibiting gold finish thicknesses of 0.254 micro-meters (10
micro-inch) or less (a.k.a. ''gold-flash'') are
exempt from this requirement.

These requirements may be eliminated if there is objective evidence
approved
by the user prior to use that there are
no gold related solder embrittlement problems associated with the
soldering
process being used.

Bob Landman
H&L Instruments, LLC 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg Owens
Sent: Thursday, February 04, 2010 5:16 PM
To: [log in to unmask]
Subject: Re: [TN] Tinning gold-plated solder cup of connectors

Dear Dave:

J-STD-001's only exception to gold tinning is ENIG plated PCBs. Also it
provides that the entire requirement be ignored if you have data to
support
that no gold embrittlement issues exist without pre-tinning. 

Gregg Owens
Technical Writer - Avionics
Space Exploration Technologies Corporation

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave He
Sent: Thursday, February 04, 2010 12:19 PM
To: [log in to unmask]
Subject: [TN] Tinning gold-plated solder cup of connectors

Does gold plated solder cup of connector need tinning per J-STD-001? Or
is
this a exemption? Thanks.

 

Best regards,

 

Dave He

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2