TECHNET Archives

February 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 2 Feb 2010 20:49:19 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Joe Fjelstad <[log in to unmask]>
Parts/Attachments:
text/plain (131 lines)
It would be helpful to know the size of the device, I/O count,  pitch and 
the location of the "lifts" (corner or edge) and the specifics of  the 
substrates, package and mounting along with process specifics for  starters. Also 
is this a one time event or a recurring one?  Right now it is just a 
curiosity  
 
As Werner has alluded with his comment that the picture is "less than  
illuminating", it seems there are still "other shoes still need to drop".
 
Kind regards, 
Joe 
 
 
In a message dated 2/2/2010 5:13:11 P.M. Pacific Standard Time,  
[log in to unmask] writes:

Hi Steve  & All,
A 'mechanical hit' would not cause this.  While the pic is  less than fully 
illuminating, I have seen similar 'buckle ups' with Pb-free  
solders/soldering before.
We need to remember, that SAC is 40% stiffer than  SnPb, has a higher yield 
strength and creeps about a factor of 50 slower—it  thus, becomes a 
mechanically significant layer with a higher CTE than Cu and  the PCB(x,y).

Werner








-----Original  Message-----
From: Steve Gregory <[log in to unmask]>
To:  [log in to unmask]
Sent: Tue, Feb 2, 2010 6:10 pm
Subject: Re: [TN] track  lifting


Hi Pearl,

Here's your  picture:

http://stevezeva.homestead.com/files/Track_Lifting.JPG

What  I see in the picture is that BGA (it is a BGA isn't it?) was  almost
ripped-off the board somehow. 

The traces are stretched and  the soldermask has been torn up from the 
board.
The root cause is that  something mechanically hit the BGA and ripped up 
pads
and traces. Is there  any other marks on the BGA?

Steve

-----Original  Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of pearl  petras
Sent: Tuesday, February 02, 2010 5:13 PM
To:  [log in to unmask]
Subject: [TN] track lifting

While we wait for IPC to  set up a picture site, could I impose on Steve to
post another  picture?
Any comments as to what could possibly be the root causes of this  is much
appreciated.  

Thanks so much


__________________________________________________________________
Yahoo!  Canada Toolbar: Search from anywhere on the web, and bookmark  your
favourite sites. Download it  now
http://ca.toolbar.yahoo.com.

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or  (MAIL)
To receive ONE mailing per day of all the posts: send e-mail  to
[log in to unmask]: SET Technet Digest
Search the archives of previous  posts at: http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional  information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100  ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or  (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to  
[log in to unmask]: SET Technet Digest
Search the archives of previous  posts at: http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for 
additional  information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------



---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2