TECHNET Archives

February 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 11 Feb 2010 14:14:00 -0500
Reply-To:
Bob Landman <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Bob Landman <[log in to unmask]>
Parts/Attachments:
text/plain (70 lines)
Excellent finds Joe.  The Engineering Disasters segment (6 minutes I think it is) is the only TV coverage Of this problem.  
I wish they'd do an update because Mike Osterman's comment (film was done in 2004) was that the industry would have a replacement for lead
by the time the ban (2006) was enacted.  I'm going to send them a comment http://www.history.com/content/modernmarvels/articles 
to let them know what's been happening since they did that segment.  Maybe they'll update it. 

Here's their contact info: [log in to unmask] 

On the same YouTube page is this video from Jay that shows how difficult it is to detect whiskers.
If the problem with even a portion of the Toyota complaints is whiskers, I don't imagine they will
Know how to detect them.

This is the video http://www.youtube.com/watch?v=8rzqkF_e9Dw&feature=related  of a small relay ~ 1993

Bob Landman
H&L Instruments, LLC 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Thursday, February 11, 2010 11:27 AM
To: [log in to unmask]
Subject: [TN] tin whisker videos

Interesting Jay Bruss from NASA has clearly done a great deal of investigating the matter.   (search   jaybrusse   on You Tube for more of his collection)

http://www.youtube.com/watch?v=kYlWjqb-Qvg&NR=1

http://www.youtube.com/watch?v=_QmBDDdXaUg



These are a series of segements to a video on the topic 

http://www.youtube.com/watch?v=pGZUdnPoU_I&NR=1

http://www.youtube.com/watch?v=o758FoVY_8w&NR=1

http://www.youtube.com/watch?v=goyWEYGKPrQ&NR=1

http://www.youtube.com/watch?v=nO-7aFZ8c3E&NR=1

http://www.youtube.com/watch?v=zvl1bR5N1U4&NR=1




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2