Graham:
This is from Wikipedia:
"Silver solder is also used in manufacturing to join metal parts that cannot be welded. The alloys used for these purposes contain a high proportion of silver (up to 40%), and may also contain cadmium."
Believe it or not, hand made steel frame racing bicycles were often silver soldered, as you don't need to heat the metal as hot, as when you braze. And the bond is STRONG.
Rudy Sedlak
--- On Thu, 2/11/10, Graham Collins <[log in to unmask]> wrote:
From: Graham Collins <[log in to unmask]>
Subject: [TN] Old reference for silver solder - what's it cross ref to?
To: [log in to unmask]
Date: Thursday, February 11, 2010, 9:42 AM
Hello Technet
I seem plagued with strange solder questions these days. Can somebody
help with a cross-reference from an old solder callout to what this
would be referred to as now? I have a drawing that references:
"QQ-S-571 alloy 94LTS Type WRAP3", and refers to it as "silver solder".
I can get the last version of QQ-S-571 (rev F, before it was cancelled
and J-STD-006 adopted), but I do not see this type of callout. Does
anyone have something that will tell me what's in this solder?
Thanks!
Graham Collins
Halifax Production Engineering
L-3 Communications ES
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|