TECHNET Archives

February 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 5 Feb 2010 22:12:53 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
From:
Bev Christian <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (719 lines)
Werner,

Oh the machines are hermetic, but most RF can are not - they have holes
through them.  So the fluids condense inside the RF can enclosure and
even if you leave circuit packs in the oven for hours on end,  you can't
get the stuff out from inside the cans, so when you take the boards
outside the oven, you lose the $$$$ fluid.

Bev

 

From: Werner Engelmaier [mailto:[log in to unmask]] 
Sent: Friday, February 05, 2010 10:09 PM
To: [log in to unmask]; Bev Christian
Subject: Re: [TN] Vapor Phase soldering

 

Bev,
Is that with any of the new machines? This would be discouraging. I
thought these new machines are pretty hermetic.
Werner

 

 

 

-----Original Message-----
From: Bev Christian <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Feb 5, 2010 8:43 pm
Subject: Re: [TN] Vapor Phase soldering

We've given up on vapor phase. The liquid condenses inside the RF cans.
Too $ to 




let evaporate outside the oven. And even if the GWP is "only" something
less 




than 100, still too high for me. 




Bev




RIM  









----- Original Message -----




From: TechNet <[log in to unmask]>




To: [log in to unmask] <[log in to unmask]>




Sent: Fri Feb 05 18:38:37 2010




Subject: Re: [TN] Vapor Phase soldering














 Hi Graham




I am looking for info on what is available to make recommendations to
clients. 




It is becoming more and more clear, that in order to avoid a manner of
problems 




caused by Pb-free soldering temperatures, the best option is to solder
with the 




lowest possible temperature, and that means using vapor phase.




Werner









 














 









 









-----Original Message-----




From: Graham Naisbitt <[log in to unmask]>




To: TechNet E-Mail Forum <[log in to unmask]>; Werner Engelmaier 




<[log in to unmask]>




Sent: Fri, Feb 5, 2010 5:45 pm




Subject: Re: [TN] Vapor Phase soldering














Hi Werner









Can you be more specific?









The best VP system that I know, is now available from REHM and based
upon the 




patents of J-P Garridel (France). This employs a discontinuous
conveyorised 




system that minimises solvent losses.









Might this be what you are seeking information about?









Regards









Graham Naisbitt - KBO









Email: [log in to unmask]




Phone: +44 (0)12 5252 1500




Web: www.gen3systems.com









On 5 Feb 2010, at 08:48, Werner Engelmaier wrote:









> Hi All,




> I would appreciate any feedback on the new vapor phase soldering ovens
that 




have recently become available.




> Werner




> 




> 




> 




> 




> 




> ---------------------------------------------------




> Technet Mail List provided as a service by IPC using LISTSERV 15.0




> To unsubscribe, send a message to [log in to unmask] with following text
in




> the BODY (NOT the subject field): SIGNOFF Technet




> To temporarily halt or (re-start) delivery of Technet send e-mail to 




[log in to unmask]: SET Technet NOMAIL or (MAIL)




> To receive ONE mailing per day of all the posts: send e-mail to 




[log in to unmask]: SET Technet Digest




> Search the archives of previous posts at:
http://listserv.ipc.org/archives




> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 









additional information, or contact Keach Sasamori at [log in to unmask] or 




847-615-7100 ext.2815




> -----------------------------------------------------









 









______________________________________________________________________




This email has been scanned by the MessageLabs Email Security System.




For more information please contact helpdesk at x2960 or
[log in to unmask] 




______________________________________________________________________









---------------------------------------------------




Technet Mail List provided as a service by IPC using LISTSERV 15.0




To unsubscribe, send a message to [log in to unmask] with following text
in




the BODY (NOT the subject field): SIGNOFF Technet




To temporarily halt or (re-start) delivery of Technet send e-mail to 




[log in to unmask]: SET Technet NOMAIL or (MAIL)




To receive ONE mailing per day of all the posts: send e-mail to 




[log in to unmask]: SET Technet Digest




Search the archives of previous posts at:
http://listserv.ipc.org/archives




Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 




additional information, or contact Keach Sasamori at [log in to unmask] or 




847-615-7100 ext.2815




-----------------------------------------------------









---------------------------------------------------------------------




This transmission (including any attachments) may contain confidential 




information, privileged material (including material protected by the 




solicitor-client or other applicable privileges), or constitute
non-public 




information. Any use of this information by anyone other than the
intended 




recipient is prohibited. If you have received this transmission in
error, please 




immediately reply to the sender and delete this information from your
system. 




Use, dissemination, distribution, or reproduction of this transmission
by 




unintended recipients is not authorized and may be unlawful.









______________________________________________________________________




This email has been scanned by the MessageLabs Email Security System.




For more information please contact helpdesk at x2960 or
[log in to unmask] 




______________________________________________________________________









---------------------------------------------------




Technet Mail List provided as a service by IPC using LISTSERV 15.0




To unsubscribe, send a message to [log in to unmask] with following text
in




the BODY (NOT the subject field): SIGNOFF Technet




To temporarily halt or (re-start) delivery of Technet send e-mail to 




[log in to unmask]: SET Technet NOMAIL or (MAIL)




To receive ONE mailing per day of all the posts: send e-mail to 




[log in to unmask]: SET Technet Digest




Search the archives of previous posts at:
http://listserv.ipc.org/archives




Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 




additional information, or contact Keach Sasamori at [log in to unmask] or 




847-615-7100 ext.2815




-----------------------------------------------------





---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2