How about creep corrosion? Some environments are harsh. A simple
rubber band can attack the finish. sulfur
Vic,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, January 11, 2010 3:11 PM
To: [log in to unmask]
Subject: [TN] Using Pressfit connectors on an Immersion Silver PWB
Has anyone experienced any issues with using pressfit connectors on a
circuit board that has Immersion silver finish? Do I need to worry about
any tarnishing inside the pressfit connector holes? Since there will be
no solder, the holes will remain open, and thus I was wondering if there
have been any issues with this.
I am considering using immersion silver as a finish for a high
reliability design, and I have never had issues using it with thousands
of medical and military and other applications, including
telecommunication blades where pressfit connectors were used. However,
this is a military application, and I want to know if there are any
potential issues before I commit to using it for this application.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|