Thanks for sharing your input. I do require a fast cure time.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Friday, January 29, 2010 1:13 PM
To: [log in to unmask]
Subject: Re: [TN] Lecoset 7007 Acrylic Cold -Curing resin
We use our cold-cure epoxy as a 65C cure. It's off label use, but gets us a very strong, hard mount in 90 minutes, totally negligible shrinkage and excellent adhesion. If 90 minutes is too long, you'll probably have to go with an acrylic.
If you're buying from someplace other than the materialography supply house, there are lots of other properties to worry about.
Chris
-----Original Message-----
From: Ian Hanna [mailto:[log in to unmask]]
Sent: Friday, January 29, 2010 2:01 PM
To: TechNet E-Mail Forum; Chris Mahanna
Subject: RE: [TN] Lecoset 7007 Acrylic Cold -Curing resin
we find that cold-cure acrylic is very good for most in-process
microsectioning. the ease of use and quick setting are very handy in a
production environment for unpopulated boards. for high-precision
work we use cold cure epoxy -- the results are more pleasing but it is a
titch less user friendly when preparing the samples...
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna
Sent: Friday, January 29, 2010 1:43 PM
To: [log in to unmask]
Subject: Re: [TN] Lecoset 7007 Acrylic Cold -Curing resin
Victor,
We've tried everything. In general you'll be much more satisfied with
epoxy results. But be careful, not all epoxy is equal. Struers has got
the good stuff, but you'll pay $$$$ If you want to try some straight
from the formulator try Axson (although if I remember correctly their
best stuff was urethanes). IF we had a reliable supply of our favorite,
I'd tell you what it is :) sorry. Chris
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Friday, January 22, 2010 8:08 AM
To: [log in to unmask]
Subject: [TN] Lecoset 7007 Acrylic Cold -Curing resin
Fellow TechNetters:
Anyone out there have experience using the about stated product for
cross section mounts. I want to use a round mount with I.D. of 1.5
inch and a 0.75 inch height.
Victor,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|