TECHNET Archives

January 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Matthias Mansfeld <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Matthias Mansfeld <[log in to unmask]>
Date:
Thu, 28 Jan 2010 08:01:47 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (97 lines)
Hello,

The numbering scheme looks like EPCOS, I assume you picked the right 
datasheet, but maybe Prashant can answer this better.

IMHO The remark on page 32 applies to normal operation.

I assume (as EPCOS writes on page 31 "Complete removal of flux is 
recommended to avoid surface contamination that can result in an
instable and/or high leakage current.") appropiate cleaning processes 
are allowed, and maybe aqueous cleaning would also work but with some 
precautions (dry bake after cleaning and before tests) In that case I 
would ask EPCOS and/or look for cleaning recommendations on their 
website.

Best regards
Matthias


On 27 Jan 2010 at 22:40, Ahne Oosterhof wrote:

> Check: http://www.epcos.com/inf/75/db/CTVS_09/Standard__CU.pdf
> Read warning on page 32.
> 
> Enjoy, 
> Ahne.
> 
> PS: All attachments are always stripped from the message in the
> TechNet. I hope I picked the correct manufacturer.
> 
> 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of prashant chopra
> Sent: Wednesday, January 27, 2010 20:34 To: [log in to unmask] Subject:
> [TN] MOV issue
> 
> Hi,
>  
> I need help on issue regarding the MOV. We are using this MOV on one
> of our PWA. This PWA goes through the cleaning process (aquawash). 
> Then the PWA is subjected to various tests.The MOV failure happens
> during a high voltage test due to hydration of device during cleaning
> process.   I am attaching the datasheet above. the Part number being
> used is CU3225K275G2K1.   Has anyone observed this before? Can anyone
> let me know what can be done to prevent this failure. (At the moment,
> we cannot stop the cleaning process during the PWA build).   Looking
> forward to comments and help.   Rgds Prashant
> 
> 
>       Your Mail works best with the New Yahoo Optimized IE8. Get it
>       NOW!
> http://downloads.yahoo.com/in/internetexplorer/
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------


-- 
Matthias Mansfeld Elektronik * Leiterplattenlayout
Neithardtstr. 3, 85540 Haar; Tel.: 089/4620 093-7, Fax: -8
Internet: http://www.mansfeld-elektronik.de
GPG http://www.mansfeld-elektronik.de/gnupgkey/mansfeld.asc

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2