With respect to my question about galvanic corrosion problems using
ImAg, I have recently discovered some info I had completely missed. On
the Anodic Chart, Silver is rated at .15V, Nickel at .30, Rhodium .05
and Gold .00. Also, for harsh environments such as outdoors, high
humidity or salt environs, there should be no more that .15V difference
in the Anodic Value, to preclude galvanic corrosion problems. So, Nickel
plated, Rhodium Plated or Gold plated hardware should be OK. Lots of
hardware can be obtained with Nickel Plate. Copper, at .35 volts might
also be considered OK for some applications.
And thanks for all the other replies concerning Class 3 and ImAg.
Chet Harner Sr. Engineer Crane Hydro-AirePO Box 7722 Burbank Ca -
91510 818-526-2600 x3557
--------------------------------------------------------------------------------
We value your opinion! How may we serve you better?
Please click the survey link to tell us how we are doing:
http://www.craneae.com/ContactUs/VoiceofCustomer.aspx
Your feedback is of the utmost importance to us. Thank you for your time.
--------------------------------------------------------------------------------
Crane Aerospace & Electronics Confidentiality Statement:
The information contained in this email message may be privileged and is
confidential information intended only for the use of the recipient, or any
employee or agent responsible to deliver it to the intended recipient. Any
unauthorized use, distribution or copying of this information is strictly prohibited
and may be unlawful. If you have received this communication in error, please notify
the sender immediately and destroy the original message and all attachments from
your electronic files.
--------------------------------------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|