Hello
I'm looking for feedback with respect to writing a PWB Laminate Specification that is tight enough to ensure consistent PWA performance and reliability; but which is also flexible enough to ensure good 'Manufacturability'.
Up until now our Fabricator has used Isola IS410, which is a Phenolic Laminate without Fillers that conforms to IPC-4101B Specification Sheets 124 and 129. I'm quite happy to approve alternative manufacturer equivalents which have the same composition and conform to the same Specification Sheets; ITEQ's IT-180 for example. However, our Fabricator has a preference for a Phenolic Laminate with Fillers, that conforms to IPC-4101B Specification Sheets 99 and 126.
Am I being overly cautious if I deny their request for change? Can anyone report any adverse experiences they have had when making this change, that I should be aware of? Are there any differences in the properties or characteristics of the two types of Laminates that I should pay particular attention to?
Thanks
James Liddle
_________________________________________________________________
Add your Gmail and Yahoo! Mail email accounts into Hotmail - it's easy
http://clk.atdmt.com/UKM/go/186394592/direct/01/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|