Good catches Steve. I've seen that segment of Engineering Disasters. Wish they would update it as it was done in 2004 and as we know, RoHS didn't kick in until 2006. Interesting that people keep forgetting that pure tin (matte or bright) will grow whiskers.
Another excellent article (with a link to a video interview of Joe Fjelstad by Dr. Howard Johnson is at this link
http://www.edn.com/article/CA6477864.html?nid=2551
Bob Landman
_____
From: stephengregory5849 [mailto:[log in to unmask]]
To: [log in to unmask]
Sent: Sat, 30 Jan 2010 16:18:49 -0500
Subject: Re: [LF] [tinwhiskers] Re: Perfect opportunity for tin whiskers induced failures
This is the article published in 2005 about the shutdown of the Millstone
nuclear powerplant from a tin whisker:
http://tinyurl.com/fvccb
Steve
_____
From: stephengregory5849 [mailto:[log in to unmask]]
To: [log in to unmask], [log in to unmask]
Sent: Sat, 30 Jan 2010 16:18:49 -0500
Subject: Re: [LF] [tinwhiskers] Re: Perfect opportunity for tin whiskers induced failures
This is the article published in 2005 about the shutdown of the Millstone
nuclear powerplant from a tin whisker:
http://tinyurl.com/fvccb
Steve
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------