Ran into that once last year again and found that this time is was caused by the solder paste being stored too cold...You know if you don't write down C some people think that means F and everything freezes...
Then you only find out about it after the solder balls...
Went back to brushing on WS609 mix and the reflow oven and things got cleared up...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of stephen gregory
Sent: Wednesday, January 13, 2010 12:24 PM
To: [log in to unmask]
Subject: [TN] Return of the "Snotballs"
Maybe some of you remember a post I made a couple of years ago when I was in Tulsa and I had a reflow problem with a SAC solderpaste. It was then I learned of a new term called "Snotballs". Here was the picture I posted back then:
http://stevezeva.homestead.com/files/Snotballs.jpg
Well guess who decided to follow me out to Pennsylvania? Check out:
http://stevezeva.homestead.com/Type_4.JPG
Same vendor, same alloy.
All I can say is make sure you know where your powder is coming from.
Steve Gregory
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
==============================================================================
This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto.
==============================================================================
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|