TECHNET Archives

January 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Mon, 11 Jan 2010 16:34:01 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (83 lines)
Hi Richard - yes, you can use an immersion silver pwb surface finish with 
a press fit connector. Two primary areas of importance; (1) team with the 
connector fabricator and make sure that the plated thru hole is designed 
specifically for the press fit connector you are going to use. In the days 
of tin/lead surface finishes, the tin/lead surface finish behaved somewhat 
like a "lubricant" during pin insertion. The immersion finish families 
(ImAg, ImSn, ENIG, ENEPIG,) are not as forgiving thus you need to may more 
due diligence to getting the plated thru hole specified accurately; (2) to 
what extent is the press fit connector going to be exposed to the use 
environment and what kind of use environment is it? As Lee Parker 
detailed, OSP/bare copper can be a very reliable under a variety of use 
environment exposures. If you are enclosed in a metal housing and you are 
using a conformal coating, then you are pretty robust to many use 
environments.  Rockwell Collins is using press fit connectors in a number 
of use environments (both military and commercial) successfully. Just need 
to do some homework as part of the early design process. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




"Stadem, Richard D." <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
01/11/2010 03:10 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D." <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Using Pressfit connectors on an Immersion Silver PWB






Has anyone experienced any issues with using pressfit connectors on a
circuit board that has Immersion silver finish? Do I need to worry about
any tarnishing inside the pressfit connector holes? Since there will be
no solder, the holes will remain open, and thus I was wondering if there
have been any issues with this.

I am considering using immersion silver as a finish for a high
reliability design, and I have never had issues using it with thousands
of medical and military and other applications, including
telecommunication blades where pressfit connectors were used. However,
this is a military application, and I want to know if there are any
potential issues before I commit to using it for this application. 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2