TECHNET Archives

January 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Mon, 11 Jan 2010 14:06:30 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Paul Edwards <[log in to unmask]>
Subject:
From:
Paul Edwards <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (64 lines)
Since you have used press-fit connectors with ImAg in other applications, then I can assume you are using press-fits designed for thinly plated Cu barrels...

But is mil apps since the environments are typically more extreme I would consider something other than ImAg... The Press-fit will cut through to the Cu and provide an exposed channel of Cu and Ag... This gives moisture a way to penetrate not only the barrel but also the solid-solid metal joint interface from the weakest plane, the sliding plane...Mechanical movement then will leverage this plane generating micro-cracks then micro-voids which in the presence of moisture and current would cause corrosion... This will lead to joint failure, or at worst case, an intermittent failure...

I would stick with solder first then Ag-Ni... 

Paul

Paul Edwards
Surface Art Engineering

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Monday, January 11, 2010 1:11 PM
To: [log in to unmask]
Subject: [TN] Using Pressfit connectors on an Immersion Silver PWB

Has anyone experienced any issues with using pressfit connectors on a
circuit board that has Immersion silver finish? Do I need to worry about
any tarnishing inside the pressfit connector holes? Since there will be
no solder, the holes will remain open, and thus I was wondering if there
have been any issues with this.

I am considering using immersion silver as a finish for a high
reliability design, and I have never had issues using it with thousands
of medical and military and other applications, including
telecommunication blades where pressfit connectors were used. However,
this is a military application, and I want to know if there are any
potential issues before I commit to using it for this application. 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


==============================================================================

This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto. 

==============================================================================


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2