Yes, it's is one of several metals used to alloy for harder cast
bullets. It's standard in lead wheelweights (which happen to be a
favorite Pb source for the do it yourself caster). Appropriate
bullet hardness is a function of pressures for a given load. Hardness
is a Goldilocks problem for the cast boolit loader.
Too soft and leading occurs at some higher velocity.
Too hard and the boolit base doesn't obturate to form a seal as it
travels through the barrel. That allows gases to escape up the lands
and flamecut the slug (leaving lead in the bore).
There are a variety of methods for coping with higher pressures and
velocities. Hardness can be increased by alloying and water
quenching. Metal gas checks (Cu or Al) can be swaged to the boolit
base. Some hard core old school loaders paper patch their cast boolit
cartridges (which has the advantage of lapping/polishing their bores).
almost certainly on a DHS list somewhere... >:-}
dw
Not me but wish I was their
neighbor... http://castboolits.gunloads.com/showthread.php?t=26559
At 08:27 AM 1/20/2010, Robert Kondner wrote:
>Hi,
>
> I recall that antimony was used in casting bullets. I recall it reduced
>"Fouling" in rifled barrels. It made the metal harder..
>
>Bob Kondner
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
>Sent: Wednesday, January 20, 2010 10:30 AM
>To: [log in to unmask]
>Subject: [TN] Antimony in solder
>
>Hi Technet
>A solder question today. What is the technical difference in using a
>solder alloy containing .2% to .5% antimony (Sn63Pb37Sb.4A) versus using
>standard eutectic SN63PB37 solder? Reliability implications? Easier to
>solder or inspect?
>
>Thanks!
>
>Graham Collins
>
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|