Is that the right number? I'm trying to look for it, but am not seeing it, at ipc.org. Maybe IPC-2612-1?
Shawn Upton, KB1CKT
Test Engineer
Allegro MicroSystems, Inc
[log in to unmask]
603.626.2429/fax: 603.641.5336
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Head
Sent: Thursday, December 10, 2009 10:48 AM
To: [log in to unmask]
Subject: Re: [TN] PCB parts that are not installed
The DNI, MO and ALT are in 9.3 of IPC-2612.
James
James Head BEng CID MIIE MIET
Senior PCB CAD Engineer
Crowcon Detection Systems Limited
2 Blacklands Way
Abingdon Business Park
ABINGDON
OX14 1DY
Telephone: +44 (0) 1235 557700 extension (9) 289
Fax: 07092024504
Email: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Upton, Shawn
Sent: 10 December 2009 15:19
To: [log in to unmask]
Subject: Re: [TN] PCB parts that are not installed
Interesting stuff all. From what I can tell (here and on another
forum), there isn't really a clear "standard" to either BOM's or this
issue. [Nor to parts that are installed after testing the assembly.]
I've seen DNI, TBD, SOT, SAT, DNA to describe these parts! It seems
that any naming convention can be used, with the knowledge that it will
have to be explained (DNI means don't install, SAT means something will
get installed at a later date, etc).
Shawn Upton, KB1CKT
Test Engineer
Allegro MicroSystems, Inc
[log in to unmask]
603.626.2429/fax: 603.641.5336
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
********************************************************
The information transmitted is intended only for the person or entity to
which it is addressed and may contain confidential and/or privileged
material. If you are not the addressee, any disclosure, reproduction,
copying, distribution, or other dissemination or use of this transmission in
error please notify the sender immediately and then delete this e-mail.
E-mail transmission cannot be guaranteed to be secure or error free as
information could be intercepted, corrupted lost, destroyed, arrive late or
incomplete, or contain viruses.
The sender therefore does not accept liability for any errors or omissions
in the contents of this message which arise as a result of e-mail
transmission. If verification is required please request a hard copy
version.
********************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|