Wandermask (2211 ) of Techspray or spot on of Multicore can do the job
You can order the PCBs with such coating
e mail: [log in to unmask]
Think green before printing this mail... Thanks
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Wednesday, December 02, 2009 9:47 AM
To: [log in to unmask]
Subject: Re: [TN] Pad that does not solder.
We use something we name 'elephant snot'. Easily removed after soldering. I will try to find what's the products real name.
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: onsdag 2 december 2009 03:14
To: [log in to unmask]
Subject: Re: [TN] Pad that does not solder.
Henry,
What about a temporary solder mask?
Bev
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue Dec 01 19:28:21 2009
Subject: [TN] Pad that does not solder.
Hi,
I have an application where I need to force a pad to not solder (or at least solder to a consistent thickness) in wave solder. The pad will eventually recieve a mechanical connection. I'm trying to design a land that will either skip, or solder to a consistent minimum thickness. The pad is large about 0.500 by 0.500. Maybe some sort of a checkerboard, or grid of vias, etc? The wave is leadfree with sac solder.
Selective soldering has already been ruled out due to other design constraints, and I'm also pursuing the idea of peelable mask.
Any ideas?
Thanks.
Henry.
__________________________________________________________________
Make your browsing faster, safer, and easier with the new Internet Explorer® 8. Optimized for Yahoo! Get it Now for Free! at http://downloads.yahoo.com/ca/internetexplorer/
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|