From:
Steven Creswick <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (163 lines)
Werner - Dale,

Here in western lower Michigan we received 6-9" of wet snow, with outside temps just below freezing.  Just the right conditions for ice formation.

With economic situations the way they are, if schools shut down, the road commissions appear to clear the roads less enthusiastically [read as - not at all in the more rural areas].

Our roads into town are literally solid ice.  One can safely travel at 40-50 mph without concern - unless one attempts a rapid change in vector, or velocity - then all bets are off!  So in the wee hours of the morning, before the grannies are up, the flow is pretty good.  After that, plan on a long slow drive.  Most people get their 'snow legs'.  Some never do, and find the ditch [or non-road surface, or object].

It is always good to remember physics!  Momentum can be a real friend when going up an icy hill, but can be nasty when reducing velocity.  It is just best to slow down and be vigilant of other drivers and conditions.


As an unpaid point of view - am trying out a set of Bridgestone Blizzak tires on the vehicles.  They seem to do VERY well on ice and snow.  Not an all-weather tire.  Rubber is too soft for running on bare roads, but sure grips well on the snow and ice!

Steve Creswick

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Friday, December 04, 2009 3:58 PM
To: [log in to unmask]
Subject: Re: [TN] test

 Dale,
Please be careful—to you it may seem 'mildly humorous,' but most folks you are sharing the road with have no clue how to drive in this stuff, particularly with bald tires.
Werner

 

 

-----Original Message-----
From: Dale Ritzen <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Dec 4, 2009 3:53 pm
Subject: Re: [TN] test


Well, it's snowing here in Austin, Texas so I'm waiting for everything to shut 
down so we can all go home. Accumulation is expected to be less than 1", and 
it'll probably melt in 20-minutes, but that's a major snow storm here in Austin. 
Being from Nebraska, I find that more than mildly humorous...

By the way... Y'all evidently passed the "test".

Dale Ritzen, CQA
Quality Manager/ISO Management Representative
Austin Manufacturing Services

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Friday, December 04, 2009 2:34 PM
To: [log in to unmask]
Subject: Re: [TN] test

 Nose to the grind stone-no golf, it is raining.
Werner

 

 

-----Original Message-----
From: Mike Buetow <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Dec 4, 2009 3:27 pm
Subject: Re: [TN] test


It's Friday afternoon. We're all hard at work. 

(haha) 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Crawford
Sent: Friday, December 04, 2009 3:22 PM
To: [log in to unmask]
Subject: [TN] test

Yeah I know--staff should know if it's working but I haven't seen any msgs in 
quite some time.

Jack Crawford, IOM
IPC Director Certification and Assembly Technology [log in to unmask]
847-597-2893
FAX  847-615-5693
3000 Lakeside Drive, Suite 309 S
Bannockburn, IL, 60015

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in the BODY 
(NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet 
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives 
of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or 
contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in the BODY 
(NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) 
delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of 
all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in the BODY 
(NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) 
delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or 
(MAIL) To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest Search the archives of previous posts at: 
http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2