Werner Engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (84 lines)
 Hi Denny,
You got it—I much rather have the snow under the shovels of my skis, then ON some shovel I have to lift. Give me 30 inches on a slope in Utah not 1 inch on the road.

Merry Christmas, 
Werner

 

 

-----Original Message-----
From: Dennis Fritz <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Dec 22, 2009 4:17 pm
Subject: Re: [TN] NTC - Merry Christmas - anyone out there?


Werner - what is "dust"?   Haven't seen anything but snow on the ground in days.  
Don't you sorely miss the white stuff in New Jersey, with the nice holiday 
traffic?  I know, I know, you want your white stuff in Aspen, or Tahoe, or 
Whistler.  



-----Original Message-----
From: Steven Creswick <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, Dec 22, 2009 10:31 am
Subject: Re: [TN] NTC - Merry Christmas - anyone out there?


Werner,
Is that like saying, "Blonds have more fun?" ...  Consultants have more
fun'?
I just thought I would scuffle my feet a bit and stir up a little dust.
ind of like poking a stick into a wasp nest - do it quick, then get out!!
     Did my duty!  
The best to you all.  Will go back to searching and leave you all alone.
Steve C

I think of the quagmire in the East caused by the weather ... and that
aused in Washington by the politicians.  At least the white stuff melts,
hereas the politicians are like a lingering cold that just won't go away.
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
dditional information, or contact Keach Sasamori at [log in to unmask] or 
47-615-7100 ext.2815
----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2