Hi, Bob
What you may want is an inert hard fill material such as diallyl
phthalate. It can withstand high temperature excursions later. There are
black underfill epoxies that fit this description and cure to a matte
dark gray/black finish. That type of underfill is available as a
snap-cure epoxy.
However, you may need to determine that whatever material you use is
compatible with whatever the material is for a particular component, and
is appropriate for the intended use environment. It may need to be a
low-outgassing filler for space use, as an example.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of bob wettermann
Sent: Monday, December 21, 2009 1:40 PM
To: [log in to unmask]
Subject: [TN] Black Top Vendor Suggestion?
Dear Technetters:
Does anyone know of a vendor of "black top" to
fill in voids left by laser "X-out" patterns in the top of an epoxy
(plastic) package ?
We are demarking an area of a device and would like to fill it in with
something other than a colored epoxy (too long to cure, cures with
glossy finish).
Regards
Bob Wettermann
BEST Inc
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|