IPC-600-6012 Archives

December 2009

IPC-600-6012@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
IPC-600-6012<[log in to unmask]>
X-To:
Date:
Thu, 31 Dec 2009 00:39:48 -0600
Reply-To:
"(Combined Forum of D-33a and 7-31a Subcommittees)" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="windows-1255"
Content-Transfer-Encoding:
quoted-printable
From:
Roberto Tulman <[log in to unmask]>
Parts/Attachments:
text/plain (13 lines)
Hello all!

The copper wrap requirement for filled holes asks for a continous copper from 
the hole to the pad. This wrap should be at least of a certain thickness.
I would like to have your oppinions about the acceptability of this wrap if it is 
built of two layers.
For example if 12 microns thickness is required, we built two 6 micron layers.
Happy New Year !