Hi Inge - sorry but that's a pwb topic I don't know much about other than
it is done as a standard process within our pwb fabrication base, it is
not the easiest thing in the world to do and if done incorrectly causes
havoc on solder joint reliability. We have a number of our pwb fabricators
that utilize the process and do a good job with it. The "fill and cap"
process became more mainstream about 3 years ago - before that it was
considered a specialized process with considerable cost implications.
Dave
Inge <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
11/07/2009 03:07 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Inge <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Solder Voids in Chip Components
Well, gentlemen,I'm still waiting for an answer on how to planarize the
via
fills before solder mounting the LGAs. Is that classified stuff?
/Inge
----- Original Message -----
From: "Bev Christian" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, November 07, 2009 9:54 PM
Subject: Re: [TN] Solder Voids in Chip Components
Dave,
I was playing devil's advocate. That is what we use too for non-thermal
ones. I am also an active member of the BTC committee.
Bev
RIM
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Sat Nov 07 15:33:44 2009
Subject: Re: [TN] Solder Voids in Chip Components
Hi Bev - the void criteria for a QFN/LGA ground/thermal pad that we use is
50% maximum voiding unless the component has specific thermal or grounding
requirements impacted by voiding phenomena. The topic is also being
discussed in the IPC BCT specification.
Dave Hillman
Rockwell Collins
[log in to unmask]
Bev Christian <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
11/07/2009 10:46 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Bev Christian <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Solder Voids in Chip Components
Inge,
You get to play with the weirdest stuff! I was referring to "normal"
cases.
Something more down to earth though is voiding in LGA/QFN central thermal
pads. What do people allow for that?
Bev
RIM
----- Original Message -----
From: Inge <[log in to unmask]>
To: TechNet E-Mail Forum <[log in to unmask]>; Bev Christian
Sent: Sat Nov 07 11:41:15 2009
Subject: Re: [TN] Solder Voids in Chip Components
There is an exception, namely when you have to do with high power chips.
We
mounted HexFets that disspated 200 Watts, and those with too much voids
simply burnt.
By the way, I got no answer from Kevin about how to planarize heat via
solder fills. Anyone?
/Inge
----- Original Message -----
From: "Bev Christian" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, November 07, 2009 5:10 PM
Subject: Re: [TN] Solder Voids in Chip Components
Correct. Or the voids are open to the surface, as Joyce K pointed out to
me.
Bev
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Sat Nov 07 11:02:58 2009
Subject: Re: [TN] Solder Voids in Chip Components
Unless there is a significant "segregation" of rather small voids at one
of
the interfaces :-)
Vladimir
SENTEC
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
-----Original Message-----
From: Bev Christian <[log in to unmask]>
Date: Sat, 7 Nov 2009 10:59:31
To: <[log in to unmask]>
Subject: Re: [TN] Solder Voids in Chip Components
Alejandro,
No there is not.
In the 10 years I was at Nortel we could never see any significant
difference between shear strength of solder joints with low voiding and
those that looked like Swiss cheese (up to 50% voiding). I am sure that
Werner will come back and rightly say that shear strength does not
necessarily equate to solder joint reliability. But I can say we never saw
chip cap problems that were traceable to the joint voids.
Bev
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Sat Nov 07 10:40:25 2009
Subject: [TN] Solder Voids in Chip Components
Hello,
Does anybody know if there is an IPC specification that describes the
amount
of solder voids allowed in a chip component solder joint? The IPC-A-610
Rev
D is specific describing the % of voids allowed for BGA's solder joints
(<25%) only but not for any other type of components.
Saludos Cordiales / Best Regards
Alejandro A. Domínguez
Robert Bosch Corporation
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from
your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be
unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|