It is related to the solder acceptance requirements listed in J-STD-001D
paragraph 4.14 and 7.6.
Same requirements are listed in IPC-A-610D.
You can achieve this with old, oxidized components, but it will be much
more difficult to do so.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani
Sent: Wednesday, November 04, 2009 3:35 PM
To: [log in to unmask]
Subject: Re: [TN] Component Shelf Life
Hello Bev, Gregg,
Thank you for getting back to me. I am curious now, how is it related to
the IPC class?
Regards,
Paymon Sani
Quality Engineer
Creation Technologies
Office: 905.754.5000 x 5363
[log in to unmask] | www.creationtech.com
-----Original Message-----
From: Bev Christian [mailto:[log in to unmask]]
Sent: Wednesday, November 04, 2009 10:20 AM
To: TechNet E-Mail Forum; Paymon Sani
Subject: RE: [TN] Component Shelf Life
Paymon,
Gregg hit it on the nail head.
In addition, it is going to depend on finish, finish thickness (varies)
and what your level of acceptability is (which IPC class product do you
build?).
I also do not know of a published, recent standard on this topic.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paymon Sani
Sent: Wednesday, November 04, 2009 9:54 AM
To: [log in to unmask]
Subject: [TN] Component Shelf Life
Dear Colleagues,
I am looking for a standard for component shelf life. Is anyone aware of
such document?
Best Regards,
Paymon Sani
Quality Engineer
Creation Technologies
Office: 905.754.5000 x 5363
110 Clegg Road | Markham, ON, Canada | L6G 1E1
[log in to unmask]<mailto:[log in to unmask]> |
www.creationtech.com<http://www.creationtech.com/>
[cid:[log in to unmask]]Working together to build the future
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|