Hi Steve,
Sorry, I have not seen the arrangement and I do not if there is sufficient strain relief.
Werner
-----Original Message-----
From: Steven Creswick <[log in to unmask]>
To: [log in to unmask]
Sent: Sun, Nov 22, 2009 7:45 pm
Subject: Re: [TN] NTC Large Hadron Collider Restarts
Steve,
I admit that I should have taken more than a quick glance at the process
document which you presented, however, if the both parts of the joint have
been pre-tinned, AND the JOINT to be soldered is indeed brought up to 230C+,
why shouldn't the joint be reasonable?
My recollection is that the Sn96.5/Ag3.5 is a eutectic solder, melting at
221C, so the 230C is certainly a whole lot closer than I would prefer to run
with, but it should indeed have melted and bonded with the pre-tinned
surfaces.
Subsequent posts have discussed tin pest, etc.
My greatest apprehension is in regard to the stresses imposed in the joint
[any joint material] when transitioning from room temp to cryogenic and back
again. I hope there is some serious stress/strain relief built into the
joint structure!
Werner, since you have had the opportunity to see the instrument to some
degree, can you provide insight as to the physical size and potential delta
length which may be involved in the soldered joint?
What are the physical sizes of the 'leads'. Are they too large to join them
with a high-power ultrasonic welder, and do away with solder altogether??
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of stephengregory5849
Sent: Sunday, November 22, 2009 1:50 PM
To: [log in to unmask]
Subject: [TN] NTC Large Hadron Collider Restarts
Some of you may have heard that the LHC (Large Hadron Collider) has
restarted after shutting down last year because of a reported bad solder
joint.
I have wondered what kind of solder was used for the connections of the
superconducting cables that failed in the LHC, I think I know now...SN96. I
also think I found out how they soldered them. Resistance soldering. Here's
the procedure:
http://tinyurl.com/yksdbt6
and another reference:
http://accelconf.web.cern.ch/AccelConf/e06/PAPERS/THPCH183.PDF
What bothers me in both of them, is that they are only heating the
connections up to 230 C. and caution not to exceed 240 C. Is that high
enough using SN96 to form a good metallurgical bond?
Steve
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|