Hi W,
Es war nicht zu beleidigen, just played with white paper ...
Inge
----- Original Message -----
From: Werner Engelmaier
To: [log in to unmask] ; [log in to unmask]
Sent: Tuesday, November 17, 2009 4:58 PM
Subject: Re: [TN] Microvia reliability vs Lead free
Hi Inge,
Bucks are green.
But you should know, nothing good is for nothing.
I take it, you work pro bono for Saab ;-)
Werner
-----Original Message-----
From: Inge <[log in to unmask]>
To: TechNet E-Mail Forum <[log in to unmask]>; Werner Engelmaier <[log in to unmask]>
Sent: Mon, Nov 16, 2009 11:14 pm
Subject: Re: [TN] Microvia reliability vs Lead free
Sure,Werner, with black payment?
/Inge
----- Original Message ----- From: "Werner Engelmaier" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, November 16, 2009 5:04 PM
Subject: Re: [TN] Microvia reliability vs Lead free
Hi Inge,
Certainly have. This is not new, and it is not very surprising.
You may be interested in my White Paper on how to design PCBs for reiability given Pb'free soldering.
Werner
-----Original Message-----
From: Hernefjord Ingemar <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, Nov 16, 2009 3:22 pm
Subject: Re: [TN] Microvia reliability vs Lead free
any relationships are described, one of which is a Curtiss-Wright report. They
ave exposed identical boards to SnPb soldering/repair and compared with same
or SACs, and found a significant difference in time to failure.
1st thermal cycle to failure
As Received 6 x 230 Celcius 6 x 260
elcius
Mean 788 443 4
That is a dramatic change in via failures. We have seen some failures recently
n ordinary double sided FR-4 boards, which were exposed to several heat
xposures in conjunction with electrical testing. Far from 260 Celcius, think
nly 125 Celcius. If we got microvia issues with only 125 C, what if we use 260
(e.g. repeated repair)?
Has anyone seen any signs of via failure due to increased heat exposure in
ractice?
nge
--------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
dditional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|