Ioan,
Right you are, but arm-chair navigation techniques are common activities for
all of us at one time or another. I don’t' think that any of us profess to
have the answers, but it is interesting to listen to the dialog nonetheless.
My brief experiences with forced, intimate-contact conductive heating
techniques showed that I could get very good joints at just above the
theoretical liquidus IIIFFF, the joint were actually at that temperature.
The key is in thermocouple selection and placement ... and of course,
temperature control.
Surely they have thousands of these joints around the collider and to have
just one fail [this time] is pretty good. Failure analysis of the joint
itself was likely not possible - I'm sure there was one fantastic light show
when the joint let go.
Since the components to be joined were supposed to have actually/really been
pre-tinned. I would have tried to eliminate the use of flux in the
subsequent joining process by using a cover gas or possibly even vacuum ....
but these guys are in a pay-grade way above me .... well, so are many
others!
Whatever makes the nuclei go around! :-)
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Sunday, November 22, 2009 9:04 PM
To: [log in to unmask]
Subject: Re: [TN] NTC Large Hadron Collider Restarts
Esteemed colleagues,
I have always considered the knowledge of Technet as my supreme source and I
have learned a lot!
But should we even think the people soldering the hadron had no idea what
they were doing? Honestly, I am not worried a bit that just anybody got this
task. I bet big scientists were involved, even if we don't know them. Let's
not forget the soldering bible has been written by a Dutch...
Regards,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer
T | 450.967.7100 ext.244
E | [log in to unmask]
W | www.digico.cc
N'imprimer que si nécessaire - Print only if you must
-----Message d'origine-----
De : Steven Creswick [mailto:[log in to unmask]]
Envoyé : Sunday, November 22, 2009 7:46 PM
À : [log in to unmask]
Objet : Re: [TN] NTC Large Hadron Collider Restarts
Steve,
I admit that I should have taken more than a quick glance at the process
document which you presented, however, if the both parts of the joint have
been pre-tinned, AND the JOINT to be soldered is indeed brought up to 230C+,
why shouldn't the joint be reasonable?
My recollection is that the Sn96.5/Ag3.5 is a eutectic solder, melting at
221C, so the 230C is certainly a whole lot closer than I would prefer to run
with, but it should indeed have melted and bonded with the pre-tinned
surfaces.
Subsequent posts have discussed tin pest, etc.
My greatest apprehension is in regard to the stresses imposed in the joint
[any joint material] when transitioning from room temp to cryogenic and back
again. I hope there is some serious stress/strain relief built into the
joint structure!
Werner, since you have had the opportunity to see the instrument to some
degree, can you provide insight as to the physical size and potential delta
length which may be involved in the soldered joint?
What are the physical sizes of the 'leads'. Are they too large to join them
with a high-power ultrasonic welder, and do away with solder altogether??
Steve C
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|